Nylon CoPA (PA6 + PA6.6) | Black

199

Product description

PolyMide™ CoPA is based on a copolymer of Nylon 6 and Nylon 6,6. The filament combines excellent strength, toughness, and heat resistance of up to 180˚C.


Does PolyMide™ CoPA requires an enclosed printer?

No, all our Nylon features our Warp-Free™ Technology which means it does not require a heated bed or heated chamber of more than 50˚C.

PolyMide™ CoPA can be printed on a 30-40˚C bed without enclosure.


Printing, Drying and Annealing Settings?

Printing Temperature: 250˚C - 270˚C

Bed Temperature: 25˚C - 50˚C

Printing Speed: 30mm/s - 50mm/s

Fan: OFF


Drying Settings: 100˚C for 6h

(Only if the material has absorbed moisture)


Annealing Settings: 80˚ for 6h


Do you need to anneal PolyMide™ CoPA?

PolyMide™ CoPA displays outstanding mechanical and thermal properties when fully crystallized. The printed part will not reach full crystallization after the printing process, an additional step is required: Annealing.

You can anneal PolyMide™ CoPA by placing your part in the oven at 80˚C for 6h.



IAI
From Riyadh

Questions you might have

‌
‌
‌‌
‌
‌
‌‌
‌
‌
‌‌
‌
‌
‌‌
‌
‌
‌‌
‌
‌
‌‌
‌